Needle Variation
Needle Variation grows a design by putting thin layers, needles, where they lower the merit function, refining every thickness, and repeating until no needle helps. Where a needle helps comes from the needle function : how fast the merit function would fall if a vanishingly thin layer of a pool material were slipped in at a given depth. Needle Automatic runs the loop on its own; Needle Manual lets you put in one needle by hand. Both use the same material pool and the same scan.
Needle Automatic
Section titled “Needle Automatic”
A generation counts only when it lowers the MF by at least 0.01 %, the fall at which each refinement inside it stops too: smaller gains would fill the layer budget with needles that stay about a nanometre thick. A needle has to go into film that is already there, so a thin stack runs out of places before it runs out of improvement; the first time the run is needle-optimal it refines copies two, four, eight and sixteen times thicker and goes on from the lowest, as a Thicker start row. If the run never beats the design it had before that, it ends on that design.
Needle Manual
Section titled “Needle Manual”
Click a point below zero to pick its position and material. Apply insertion puts the needle in at d_new, which starts where the same line search as Needle Automatic puts it. With Refine after insert on, SQP then refines the stack for up to Refine iterations steps, with the MNT and MXT rows in force. The plot shows every point it computed, including splits that would leave part of a layer below Min thickness.
Computed quantities
Section titled “Computed quantities”- P, the needle function: the slope of the merit function for a needle of one pool material at one depth, as its thickness goes to zero. Below zero, a needle there lowers the MF.
- MF: the merit function of the Merit Function Editor; OMF, the same without the thickness rows
TT,STR,MNTandMXT. - ΔMF: in Accepted Improvements, the change from the best design before the row. TOT: the total physical thickness, nm.
- Top Designs: the generations that no other generation beats on both layer count and MF.
Controls and settings
Section titled “Controls and settings”Run, Stop, Reset, Best, Clear history: Stop pauses, shows the last design the run accepted, and the next Run carries on from it in the same run. Reset undoes the last Run press. Best puts the lowest-MF generation on the design, as Restore does for any row. Clear history forgets the rows and keeps the design.
Material Pool: the pool of materials Needle is allowed to insert. The pool starts with only the materials of the design’s layers ticked, front and back; the substrate and the media are listed under This design but unticked, and no other catalog is ticked. All / Clear select or empty the pool in one click. Once you change the pool, the window keeps your choice for every design, except that each design’s substrate and media stay unticked until you tick them on that design; a pool emptied with Clear starts again from the design’s own materials the next time the window opens.
Max layers: no new cycle starts once the stack holds this many layers. 60 by default.
Target MF: stop once the MF falls below this value; 0 runs until the design is needle-optimal.
Smart starting design: start from the best of the design and the quarter- and half-wave antireflection designs built from the pool, each refined first. Off by default.
Needle δ (nm) (Probe δ in Needle Manual): the probe needle for the rows has no exact slope for, and for the cases where the exact scan does not run. 0.5 nm by default.
Min thickness (nm): the thinnest a needle starts, the floor during refinement, and the smallest part a split layer may leave; 1 nm by default. Keep it there while synthesizing and raise it to your manufacturing minimum only in a later Refinement and Design Cleaner pass, so a manufacturable floor does not hold synthesis back. A note under the field shows when an MNT row differs.
Refine iter / gen: the most refinement steps after each insertion. 60 by default.
Synthesis refiner: the method that refines after each insertion; Trust-region Newton by default for Needle, which ended lower than Conjugate Gradient on most of the benchmark’s cases. See Optimization Methods.
Candidate search: how many batches a cycle tries before the design counts as needle-optimal: Fast one, Balanced two (the default), Thorough all.
Needle sensitivity: drop candidates whose predicted fall is under 1 %, 5 % or 15 % of the strongest in the scan; Off by default. It trims the list before the batches are taken.
Threads: how many candidates a batch holds and refines at once; the result depends on it. The default comes from the computer’s cores, so a run repeats on another computer only at the same Threads.
Profile pts / layer, Side, Refine after insert, Refine iterations: Needle Manual’s points inside each layer (16), the face it scans when Surface is Both, and the refinement after an insertion (on, 80 steps).
Needle Automatic leaves out the MNT and MXT rows, so run Refinement afterwards; Needle Manual leaves them out of its scan and starting thickness only. A PPEF row, and any math row that reads it, is left out too: its gradient comes from only the two wavelengths where the error is highest and lowest, and the needle search stalls on that. A note under Settings says so, and a Refinement run afterwards brings the peak-to-peak error down.
How it is computed
Section titled “How it is computed”Merit function
Section titled “Merit function”is the miss of row , its weight, its scale and the weight sum. The scan and the starting-thickness search use the OMF; the refinement and the 0.01 % rule use the MF. On a design with environments, is the mean of the environments’ , and the scan adds up their slopes the same way.
Needle function
Section titled “Needle function”In TFStudio’s convention , (see the conventions), the layer matrix is Macleod’s Eq. 2.111 with the sign of reversed:
A needle of material at depth splits the stack into the matrix product above it, , and the vector below it, ; for small thickness its matrix is the identity plus times its derivative:
With an absorbing incident medium has one more term, in . Each row’s slope follows by the chain rule the refinement uses for a layer thickness, and is the slope of the merit:
This is the limit of Sullivan and Dobrowolski’s pre- and post-matrix needle, and the first coefficient of Tikhonravov et al.’s series ; every material at every position is its own candidate. Rows with no exact needle slope, such as phase, group delay and the ellipsometric rows, are compared with and without a needle of thickness . Where the exact scan does not run, on a bare substrate or with Surface at Front or Back and Ignore other side off (Surface & Evaluation Modes), .
Polarization, angle and cone
Section titled “Polarization, angle and cone”is in units of the free-space admittance and is the real index of the incident medium. A row averaging s and p, or scored over an illumination cone (Design Editor), averages the slopes with the same weights it averages R, T or A. With Surface at Both, the slope goes through the incoherent sum of the two faces and the substrate, and with Symmetric (back = front) a needle goes into both faces, so the two slopes add.
Starting thickness, refinement and acceptance
Section titled “Starting thickness, refinement and acceptance”is the thickness of the layer being split, is Min thickness, is Refine iter / gen and counts refinement steps.
Tikhonravov et al. give a new layer whatever thickness lowers the merit most. Here the search stops at 60 nm: over a wide range the merit of a held stack has many minima, and a thick slab found that way can lower it while spoiling the design; refinement grows the needle afterwards. Sullivan and Dobrowolski remove the layers refinement leaves below a set thickness; a refiner with a floor parks them on it instead, so their removal is judged as Tikhonravov et al. judge it in gradual evolution: take them out, refine, and keep the result only if the merit is no worse.
References
Section titled “References”- H. A. Macleod, Thin-Film Optical Filters, 5th ed., Eq. 2.111 (layer matrix), Eqs. 2.123-2.125 (reflectance and transmittance), §2.6.4 (the two faces of a substrate), Chapter 3 (automatic design and the needle variation method).
- B. T. Sullivan and J. A. Dobrowolski, Appl. Opt. 35, 5484 (1996): the numerical needle with pre- and post-matrices.
- A. V. Tikhonravov, M. K. Trubetskov and G. W. DeBell, Appl. Opt. 35, 5493 (1996): the needle function and the synthesis loop.
- A. V. Tikhonravov, M. K. Trubetskov and G. W. DeBell, Appl. Opt. 46, 704 (2007): total optical thickness and gradual evolution.